Features:
UNS Number N06600
Inconel 600 has a excellent corrosion & high temperature resistance. Meanwhile, Inconel 600 has a high strength and good fabricability. It resists chloride-ion-incurred stress corrosion cracking, sulfur compounds and oxidizing conditions at high temperatures.
Applications:
Inconel 600 is applied in Chemical process industry, heat treating fixtures, airframe components and nuclear reactors.
Forms of Inconel 600 Available
• Sheet
• Plate
• Bar
• Pipe & Tube (welded & seamless)
• Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)
Inconel 600 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
P |
S |
|
600 |
Min. |
72 |
14 |
6 |
|
|
|
|
|
|
|
Max. |
|
17 |
10 |
0.15 |
1 |
0.5 |
0.5 |
0.015 |
0.015 |
Inconel 600 Physical properties:
|
Density |
8.4 g/cm³ |
|
Melting Point |
1370-1425 ℃ |
Inconel 600 Alloy m inimum Mechanical properties in the room temperature:
|
Aolly status |
Tensile strength |
Yield strength |
Elongation A 5 % |
Brinell hardness HB |
|
Annealing treatment |
550 |
240 |
30 |
≤195 |
|
Solution treatment |
500 |
180 |
35 |
≤185 |
ASTM Specifications
|
Pipe Smls |
Pipe Welded |
Tube Smls |
Tube Welded |
Sheet/Plate |
Bar |
Forging |
Fitting |
|
B167 |
B517 |
B163 |
B516 |
B168 |
B166 |
B564 |
B366 |